Most leaking joints are not caused by the sealant itself. They come from the wrong joint shape, poorly prepared joint faces, or sealant stuck to the bottom of the joint. Get those right and almost any good sealant will last.
1. Pick the sealant for the job
| Where | UNISEAL® product | Why |
|---|---|---|
| General building joints, precast, parapets, floors | UNISEAL® PU | One-component polyurethane, no mixing, paintable |
| Higher-movement building and precast joints | UNISEAL® PU PRO | Fast-curing PU, Class A, ±25% movement (per TDS) |
| Water-retaining structures, treatment plants, chemical areas, pavements | UNISEAL® PS | Two-component polysulphide, chemically curing, non-slumping |
| Water works, tanks, pools, rainwater systems | UNISEAL® MS Polyether | One-component MS polymer formulated for water works |
| Roads, runways, toll plazas, bridge joints | UNISEAL® Bituflex | Hot-poured rubber bitumen, no primer required |
| Fire-rated floor and wall joints | UNISEAL® VT-629 | 4-hour fire rating to BS EN 1366-4 (per TDS) |
2. Get the joint shape right
- For joints wider than 12 mm, our details use a sealant width : depth = 2 : 1. A 20 mm wide joint gets about 10 mm of sealant depth. Too deep and the sealant cannot stretch; too shallow and it tears.
- Tool the surface slightly concave so the sealant is thinnest in the middle.
- On roads, hot-poured Bituflex is finished slightly below the surface so traffic does not drag it out.
3. Use a backer rod (or filler board) underneath
The backer rod sets the sealant depth and stops the sealant bonding to the joint base:
- Choose a UNIFLEX® PE backer rod 10–20% wider than the joint, so it stays in compression.
- Push it in to the correct depth without puncturing it.
- Over UNIFLEX® PE filler board you do not need a backer rod or bond breaker tape. Over cork (RBCF) or bituminous fibreboard (FB), use bond breaker tape.
4. Prepare, prime, then seal
Clean, dry, sound joint faces, free of laitance, dust and oil. UNISEAL® Primer is required on porous faces (concrete, mortar, masonry), in joints that will be immersed in water and in fire-rated VT-629 joints; on dry, sound, non-porous joints it is optional. Brush it on both faces, let it dry 1 to 2 hours (re-prime if you do not seal within 3 hours), then gun the sealant in and tool it.
5. Avoid three-sided adhesion
If the sealant bonds to the two faces and the bottom of a groove, it cannot stretch and it will split. In sealed grooves over construction joints or induced cracks, put bond breaker tape in the groove base.
Send us the joint width, the movement and where it is (tank, road, building) and we will recommend the UNISEAL® product and backer rod size.
Typical guidance only – not an engineering design. Joint layout, sizes and reinforcement are designed and approved by the project engineer. Refer to each product's TDS.