An expansion joint filler board does two jobs. It forms the joint gap when the second pour is cast against the first, and it stays in the joint as a compressible filler, so the concrete can expand without spalling and the sealant on top has something to sit on.
All four UNIFLEX® boards do that. The differences are what they are made of, how they behave with water, and whether the joint needs a fire rating.
The four options
| Board | Made of | Best for |
|---|---|---|
| UNIFLEX® PE Filler Board | Closed-cell polyethylene: non-absorbent, bitumen free, rot proof, semi-rigid | The general choice, including water-retaining structures, basements, tanks, roads and bridges. It also acts as a natural bond breaker for the sealant. |
| UNIFLEX® FB Bituminous Fibreboard | Wood fibre impregnated with bitumen | Roads, pavements, kerbs, aprons and general concrete joints where a traditional fibreboard is specified. |
| UNIFLEX® RBCF Resin Bonded Cork | Granulated cork bound with a synthetic resin | Water tanks, treatment plants, pools and driveways where a cork filler is specified. Low load transfer across the joint. |
| UNIFLEX® PE FR Fire Retardant | Fire-retardant closed-cell PE | Fire-rated joints and partition walls, used with a fire-rated sealant. |
Our recommendation: UNIFLEX® PE
For most expansion joints we recommend UNIFLEX® PE Filler Board over fibreboard or cork:
- No bitumen, so nothing bleeds out to stain the concrete, paving or finishes in hot weather.
- Closed-cell and non-absorbent, rot proof and suitable for water-retaining structures.
- Its own bond breaker, so no tape is needed under the sealant.
- Usually lower cost than cork, which is a natural product made from the bark of the cork oak.
If your specification names bituminous fibreboard (often to ASTM D1751) or cork (often to ASTM D1752), ask the consultant to approve UNIFLEX® PE as an alternative before ordering. We can provide the TDS for the submittal.
Do I need bond breaker tape?
The sealant should stick to the two joint faces only, not to the bottom of the joint (no three-sided adhesion), or it tears when the joint opens.
- UNIFLEX® PE and PE FR: closed-cell PE does not bond to the sealant, so no bond breaker tape is needed.
- UNIFLEX® RBCF cork and UNIFLEX® FB fibreboard: put bond breaker tape on top of the board before sealing.
How it goes together
- Fix the filler board to the face of the first pour, full depth of the joint.
- Cast the second pour against it.
- Cut back or remove the top of the board to form the sealant groove, prime the faces with UNISEAL® Primer, and apply UNISEAL® sealant. For joints wider than 12 mm our details use a width-to-depth ratio of 2:1.
- For water-retaining structures the joint usually also has a centre-bulb waterstop. See how to choose a waterstop.
Fire-rated joints
For a fire-rated floor or wall joint, our typical detail uses UNIFLEX® PE FR in the core with UNISEAL® VT-629 fire-rated sealant gunned directly onto the board at each face (no backer rod – a standard backer rod is not fire rated), primed with UNISEAL® PRIMER and sealed on both faces for the 4-hour rating in 20 – 50 mm joints. Always follow the tested system on the fire certificate for the joint width and rating required.
Tell us the joint width, the depth and what the structure is (road, tank, building) and we will recommend the board thickness and send the TDS.
Typical guidance only – not an engineering design. Joint layout, sizes and reinforcement are designed and approved by the project engineer. Refer to each product's TDS.