Concrete slabs on the ground shrink as they dry and move with temperature. Joints let that happen in a straight line where you choose, instead of as random cracks. An industrial floor or pavement normally has three kinds. The engineer sets the joint layout, spacing and depths; this guide explains what goes in each.
1. Expansion (isolation) joints
A full-depth gap that lets slabs expand, typically at walls, columns, and between large bays.
- UNIFLEX® PE filler board, full depth, fixed to the first pour.
- Dowel bars at mid-depth, parallel to the surface and square to the joint, supported on chairs during the pour. One half is bonded in the first pour; the other half is debonded.
- UNIJOINT rubber dowel cap over the full debonded half, closed end, leaving a movement gap at the dowel end. It restrains vertical movement so the slabs do not settle under traffic, while allowing the joint to expand and contract.
- UNICOAT Bitumen 300 on the debonded half of the dowel to stop it bonding.
- Sealant on top: UNISEAL® PU (primed, width : depth 2 : 1) for floors, or UNISEAL® Bituflex hot-pour for roads.
- Put all dowel caps on the same side of the joint.
2. Contraction (control) joints
These create a weak line so the shrinkage crack forms there, not across the panel.
- Sawn joint: saw cut as soon as the concrete allows, to the depth set by the engineer. The crack forms under the cut. Seal with UNISEAL® sealant on backer rod, or hot-poured Bituflex on pavements.
- Crack inducer instead of sawing: UNIJOINT CI-T 30 or CI-T 50 pressed into the fresh concrete on a string line, top flush with the surface, or CI-B 75 set upright on the lean concrete. As a rule of thumb the inducer depth should be at least a quarter of the slab thickness; the consultant confirms it.
- Dowelled contraction joints use the same dowel and dowel cap arrangement as above.
3. Construction joints
The joint where one day’s pour stops and the next begins.
- In most floors it is formed square and treated like a contraction joint (dowelled and sealed).
- In water-retaining slabs and basements, add a waterstop. See how to choose a waterstop and swelling vs PVC waterstop.
Common mistakes
- Dowels not parallel to the surface or not square to the joint lock the slabs together, and they crack beside the joint.
- Sawing too late: the slab cracks by itself first.
- Sealant bonded to the bottom of the groove (three-sided adhesion) tears when the joint opens.
Send us the slab thickness, joint layout and dowel size and we will put together the filler board, dowel cap, crack inducer and sealant list, with the matching CAD details.
Typical guidance only – not an engineering design. Joint layout, sizes and reinforcement are designed and approved by the project engineer. Refer to each product's TDS.